Equilibrium between Slag and Molten Iron in the Direct Alloying of Steel with Nb2O5-Bearing Slag
Equilibrium between Slag and Molten Iron in the Direct Alloying of Steel with Nb2O5-Bearing Slag
-
摘要: Equilibrium between slag and molten iron at 1600℃ was investigated for the direct alloying of steel with Nb2O6-bearing slag. The activity of niobium oxide in the slag was measured. The αNb2O5 is in the range of 10-2-10-4. TheδNb2O5 is ranged in 100-10-2.Niobium partition decreases with the increase ofSi% and CaO/SiO2. When α0 and ΣFeO decrease, niobium partition decreases too. The δNb2o5 and the ratio of γsiO2 to γNb2O5 decrease with the incre-ase of slag basicity. The suitable thermodynamic conditions in direct alloying of steel with Nb2O5-bearing slag have been found.Abstract: Equilibrium between slag and molten iron at 1600℃ was investigated for the direct alloying of steel with Nb2O6-bearing slag. The activity of niobium oxide in the slag was measured. The αNb2O5 is in the range of 10-2-10-4. TheδNb2O5 is ranged in 100-10-2.Niobium partition decreases with the increase ofSi% and CaO/SiO2. When α0 and ΣFeO decrease, niobium partition decreases too. The δNb2o5 and the ratio of γsiO2 to γNb2O5 decrease with the incre-ase of slag basicity. The suitable thermodynamic conditions in direct alloying of steel with Nb2O5-bearing slag have been found.