新型高性能铁基超微晶软磁合金

New Ultrafine Crystalline Fe-base Soft Magnetic Alloy with Superior Propeties

  • 摘要: 本文研究了Fe73.5Nb3Cu1Si13.5B9新型高性能铁基超微晶软磁合金的性能与结构特征。结果表明,该合金的最佳退火温度为535℃,其起始磁导率μ(0.08A/m)=14.8×104,矫顽力Hc=0.6A/m,饱和磁感B(800A/m)=1.22T。最佳铁损分另为P5·10k=5.6W/kg,P5·20k=17.4W/kg,P5·50k=80W/kg,P5·100k=270W/kg。且在相当宽的频率范围内具有高有效磁导率μ'1X射线衍射分析表明.合金中主相为xFe-Si固溶体,晶粒尺寸约为11nm,点阵参数a0为0.2837nm。

     

    Abstract: The properties and microstructure of Fe73.5Nb3Cu1Si13.5B9 new ultrafine crystalline soft magnetic alloy have been investigated.The results have been shown that the alloy is combined with high relative initial permeability of μ(0.08A·m)=14.8×104. low coercivity of Hc=0.6A/m. high saturation magnetic flux density of B800A·m,=1.22 T under the optimum performance with annealing at 535℃, the optimum values of core loss have reached P5·10k=5.6W/kg, P5·20k=17.4W/kg, P5·50k=80W/kg. P5·100k=270W/kg. The alloy has high effective permeability μ'1 in a considerable wide frequency range. The microstructural analysis under X-ray diffraction was detemined that the main crystalline phase in the alloy is xFe-Si solid solution which has ultrafine grain size of d=1 1nm. lattice parameter of a a0=0.2 837nm.

     

/

返回文章
返回