Precipitation of α'-Phase in Fe-Cr-Al Alloy during Thermal Cycling Process

  • 摘要: 通过1200℃缓冷至室温热循环过程,由于铬组元非平衡偏聚,加快铬在Fe25Cr5Al合金中向晶界扩散,并产生富铬的α'相沿晶及晶内沉淀;相变导致合金脆化,在晶界可观察到微米级α'相,并产生穿晶解理断裂失效破坏。

     

    Abstract: By thermal cycling treatment from 1200℃ to room temperature, a considerable acceleration of Cr diffusion to grain boundaries in Fe25Cr5Al alloy occurred due to nonequilibrium Cr element segregation, and resulted in the precipitation of Cr-rich α'-phase at grain boundaries and within grains; micrometer scale of α'-phase was observed at the grain boundary, the phase transformation resulted in the failure of the alloy by a mode of transgranular deavage fracture.

     

/