低应变速率下锰硫比对低碳钢高温塑性的影响
Effect of the Mn/S Mass Ratio on the High Temperature Ductility of the Low Carbon Steel under Low Strain Rate
-
摘要: 研究了在低应速率(10-3/m)下锰硫比对低碳钢高温塑性的影响,实验结果表明,不同测试温度下锰硫比对钢的高温塑性的影响不同。按其影响规律,可分为4个温度区域即:(1)1350~1400℃,锰硫比越高,塑性越差;(2)1000~1350℃,锰硫比对塑性无影响;(3)800~1000℃,锰硫比越高,塑性越好;(4)600~800℃,锰硫比越高,塑性越差,同时还对锰硫比对高温塑性的影响机理进行了分析。Abstract: The effect of the Mn/S mass ratio on the high temperature ductility of the low carbon steel under low strain rate was researched. The result of the experiments shows that the Mn/S mass ratio has different effect on the high temperature ductility of steel under different temperatures. The effect can be classified into four categories:(1)1 350~1 400℃, the greater the Mn/S mass ratio is, the poorer the ductility is; (2)1 000~1 350℃,the Wn/S mass ratio has no effect on the duchlity; (3)800~1 000℃, the greater the ratio of the Mn versus S is,the better the ductility is; (4)600~800℃, the greater the mass ratio of the Mn versus S is, the poorer the ductility is. The mechanism of the effect of the Mn/S mass ratio on the high-temperature ductility is also analyzed.