不锈钢氧化法脱磷的热态模拟

Thermodynamic Simulating for Oxidizing Dephosphurization of Stainless Steel

  • 摘要: 在热力学计算的基础上,利用10kg感应炉模拟电弧炉进行了不锈钢脱磷试验,讨论了不锈钢脱磷的工艺要点,建议温度为1600℃的水平时,脱磷碳含量应大于1.55%.

     

    Abstract: Based on thermodynamic calculations, the simulating tests on dephosphurization of stainless steel were carried out. The key points of the De-P process were analyzed. It is suggested that the C be kept above 1.55% in the De-P process.

     

/