Al5Ti1B中间合金细化剂研制及同类产品对比

Manufacture of Al5TilB master alloy refiner and its comparison with other products

  • 摘要: 利用氟盐铝热反应法制备了Al5Ti1B中间合金细化剂,制定出完整的工艺路线和参数,并对其反应过程和原理进行了分析.制取的中间合金化学成分(质量分数)为:Ti,4.64%;B,0.84%.通过与荷兰KBM、英国LSM、国内某厂生产的同类产品进行化学成分、微观组织和细化效果三项指标对比分析,结果表明:自行开发的中间合金细化剂质量优于国内同类产品;同等条件下细化效果(TiAl3<50μm,TiB2<1μm)与KBM公司的同类产品接近,达到进口同类产品水平.

     

    Abstract: Al5Ti1B master alloy refiner was prepared by the reaction of complex halide salts with molten aluminum at high temperature. The manufacture process and parameter range were regulated and the principle and course of the reaction were analyzed. As for the self-made master alloy, the Ti content reaches 4.64%, and B 0.84%. The self-manufactured product was compared by comprehensive evaluation with the products manufactured by KBM, LSM and some national organization. It is found that TiAl3 particles are less than 50 μm, and TiB2 less than 1μm in the Al5Ti1B master alloy developed by Tsinghua University and Baotou Aluminum Plant. Its refining performance is closed to KBM's Al5Ti1B. The self-manufactured product reaches the international standard in composition, microstructure and refinement effect.

     

/

返回文章
返回