  • 摘要: 针对鞍钢炼钢厂"铁水预处理→LD→LF→VD→CC"X70生产流程,采用系统取样,综合分析的方法,对LF处理前后、VD处理前后、中间包、结晶器和铸坯中的TO、显微非金属夹杂物的类型、数量及尺寸分布进行了系统研究.研究结果表明:(1)铸坯中TO的平均值为17.33×10-6,铸坯中显微夹杂物数量为2.40mm-2;(2)LF处理前后钢水中显微非金属夹杂以长条及块状的Al2O3夹杂和球块状的硅酸盐夹杂为主,VD钙处理后,没有观察到纯的MnS夹杂与纯的Al2O3夹杂;(3)结晶器钢水、铸坯中有纯Al2O3夹杂再现;(4)钢中的氧化物及硫化物夹杂均没有达到完全变性的要求.

     

    Abstract: Using systematic sampling and comprehensive analysis, the variation of total oxygen content and amount, dimension and distribution of nonmetallic inclusions were studied systematically during the production process of hot metal pretreatment-LD-LF-VD-slab CC in Angang. The results show that:(1) The average total oxygen content of slab is 17.33×10-6 and the number of micro inclusions is 2.40 mm-2; (2) Before and after the LF process, micro nonmetallic inclusions in the steel are mainly strip or block Al2O3 and global or polyhedral silicate;after calcium treatment in VD, the pure brittle Al2O3 inclusions and harmful MnS inclusions along boundaries were not found; (3) The reappearance of Al2O3 inclusions in mold and slab indicates that secondary oxidation happens in the tundish or mold; (4) Oxide and sulfide inclusions are not modified fully.

     

/

返回文章
返回