轧制复合生产特厚板工艺

Production of heavy-gauge steel plates by clad rolling process

  • 摘要: 采用Q345连铸坯料,经过表面清理、焊接组坯和抽真空至1×10-3 Pa后密封,分别采用两阶段控轧和再结晶型控轧两种轧制工艺进行轧制.用剪切、拉伸和冷弯试验检验复合板的力学性能,利用扫描电镜观察分析复合板的组织与结合面.结果表明:两种轧制工艺生产出的钢板各项力学性都能达标;再结晶控轧工艺比两阶段控轧工艺复合效果更好,并生产出的钢板厚向性能更加均匀.试验条件下的轧制复合包含机械啮合与再结晶两种机制.

     

    Abstract: After surface cleaning,weld combining and vacuumizing to 1×10-3 Pa,Q345 continuous casting slabs were processed by conventional control rolling(CCR) and recrystallization control rolling(RCR).The mechanical properties of the clad rolling plates were tested by shear,tensile and cold bending tests,and the microstructures and combining boundaries were observed by scanning electron microscope(SEM).The results show that the mechanical properties of the clad rolling plates produced by the two rolling processes are all qualified.Compared with CCR process,RCR process provides a better bonding effect and the plate has better property homogeneity in the thickness direction.The clad rolling process in the experimental condition involves the mechanical meshing mechanism and the recrystallization mechanism.

     

/

返回文章
返回