冷却速度对La脱氧钢中晶内铁素体形成的影响

Effect of cooling rate on intragranular ferrite formation in La deoxidized steel

  • 摘要: 采用光学显微镜、带能谱的扫描电子显微镜等分析技术观察了不同冷速下La脱氧钢的显微组织,并绘制了静态连续冷却转变图.实验结果发现,在4~10℃·s-1的冷速范围内,钢中会有大量晶内铁素体形成,其中在8℃·s-1冷却时可以获得大量细小且弥散分布的晶内针状铁素体.La脱氧钢中含La夹杂物与α-Fe相有较低错配度,其中La2O2S夹杂物与α—Fe相的品格错配度最小为0.2%,钢中含La夹杂物均可诱导晶内针状铁素体形核并可促进感生形核.进而细化组织.

     

    Abstract: The microstructures of La deoxidized steels obtained at different cooling rates were investigaled by optical microscopy and scanning electron microscopy coupled to an energy dispersive X-ray spectrometer. The continuous cooling transformation diagram of the tested steel was also drawn in this paper. It is found that in the cooling rate range of 4 to 10℃·s-1, intragranular ferrite can form in the steel. While at the cooling rate of 8℃·s-1, the microstructure mainly consists of fine and dispersed intragranular acicular ferrite (IAF). The lattice disregistry between lanthanum-containing inclusions and α-Fe is small; especially, this value of La2O2S is 0.2%. These kinds of inclusions can induce IAF nucleation and sympathetic nucleation, and also make grains refined.

     

/

返回文章
返回