The hydrogen embrittlement (HE) sensitivity and the HE fracture characteristics of cold drawn 05Si2 martensite-ferrite (F + M) dual-phase steel were investigated. It's found that, (a) HE sensitility first increases with the area reduction by cold drawing and then turns to decreases; (b) HE of ferrite matrix plays an important role in the HE fracture.