Solubility in citric acid of dephosphorization slags from high phosphorus hot metal refining
-
-
Abstract
Consulting a practical dephosphorization slag in the converter, samples with different levels of F, P2O5, FeO, MgO and basicity were prepared in laboratory, and the effect of composition on their solubility in citric acid was analyzed by chemical analysis methods. The results show that when the slag contains fluorine, P and F mainly form fluorapatite, and the solubility in citric acid of the slag sharply decreases when the fluorine content increases in the slag. if there is no any fluorine in the slag, the solubility in citric acid can be reached up to 92.5%, but when the mass fraction of fluorine in the slag reaches to 0.5%, the solubility in citric acid drops to less than 50%. The solubility in citric acid is improved with the increase of basicity, for increasing Ca2+ can destroy the Si-O network structure. With the increase of MgO content, the solubility in citric acid increases since in the process of cooling, Mg2+ inhibits the precipitation of β-Ca3(PO4)2 crystals in which P can not be dissolved easily in the 2% citric acid. The solubility in citric acid decreases with the increase of P2O5 content, for P5+ is formed as PO43- complex ions with O2-, P5+ locates in intensive gaps formed by O2-, and the complex ions can not dissolved easily in the 2% citric acid. The solubility in citric acid will be decreased with the increase of FeOn.
-
-